Silicon oxide (SiO , 0 < x < 2) thin films have been prepared by the plasma enhanced CVD of gaseous silane and nitrous oxide (flow rate ratio 2/1) onto quartz and silicon wafer substrates at 2500C. The samples were then annealed in ambient oxygen at 100 to 6000C at intervals of 100 degrees. The Si-O-Si bending and stretching, Si-H stretching and Si-OH stretching modes were identified from the infrared spectra. The annealing process resulted in an excess of tetrahedral Si04 units and the generation of dangling bonds.

Downloads

Download data is not yet available.

Article Details

How to Cite
Tan, K., & Muhamad, M. (2017). The bonding modes and optical characteristics of annealed silicon oxide thin films prepared by plasma enhanced CVD. Malaysian Journal of Science, 16(2), 13–16. Retrieved from https://mjlis.um.edu.my/index.php/MJS/article/view/4787
Section
Original Articles